1. Sauƙaƙe da pretreatment hanyoyin kafin aluminum profiles anodizing, kamar yadda hadawa degreasing, cire halitta hadawan abu da iskar shaka fim da kuma haskaka uku ayyuka, da aluminum profiles za a iya anodized kai tsaye bayan pretreatment.
2. Tare da abũbuwan amfãni na ƙananan farashi, ƙananan amfani da aluminum, mai sauƙin aiki da aikin haske.
Ƙarar Gyaran Zazzabi | Ruwa |
25-35g/L | Ma'auni |
Ƙarar Gyaran Zazzabi | Lokaci | Zazzabi | Amfani |
20-50g/L | 2 ~ 4 min | Yanayin dakin | 5-7kg/T |
1.Don ƙayyade ƙaddamarwar FL-01 kuma kiyaye shi a cikin kewayon yanayin aiki, sake cika cikin lokaci.
2.Za fi kyau cewa bayanan bayanan aluminum yakamata suyi sau daya kafin aiwatar da kayan aikin aluminum da impurities da kara yawan amfani da marin zazzabi.
3.Ya kamata a tsaftace wanka akai-akai yayin samarwa saboda akwai wasu abubuwa marasa narkewa kamar sundries na inji da ƙura.
Ƙarar ɗanɗanon gogewar zafin jiki an cika shi da ganga filastik da aka rufe, net 30kg kowace.
Ƙananan zafin jiki polishing nutse--hanyar tantancewa
Abubuwan da ake buƙata: 1N NaOH daidaitaccen bayani ② 1% alamar phenolphthalein ③ Potassium
① Daidai pipette 20mL na maganin wanka a cikin flask conical 250mL, ƙara 50mL na ruwa mai narkewa, sannan ƙara 2 zuwa 3 saukad da na 1% phenolphthalein nuna alama, da titrate tare da 1N NaOH har sai da bayani ya canza daga launi zuwa ruwan hoda, wanda shine ƙarshen batu. .Rubuta V1 ba tare da dusashewa a cikin 30s ba.
②Ai dai dai pipette 5mL na maganin sink a cikin flask conical 250mL, a zuba 50mL na ruwa mai narkewa, ƙara 3g na potassium fluoride, narke kuma girgiza sosai, ƙara 2 zuwa 3 digo na 1% phenolphthalein, da titrate tare da 1N NaOH har sai da maganin. Mara launi zuwa ruwan hoda shine ƙarshen ƙarshen, kuma ana yin rikodin V2 idan launi bai shuɗe cikin 30s ba.
lissafta
wurin aiki (yawan maki) = 9.8 × V 1 × N
Acid kyauta ((g/L)=9.8×V 2 ×N
wurin aiki | free acid | zafin jiki |
90~130 | 20-35g/L | 18-25℃ |